Standard Test Methods for Chemical Analysis of Thermal Insulation Materials for Leachable Chloride, Fluoride, Silicate, and Sodium Ions
适用范围:<p>Research has demonstrated that in addition to the halide ion chloride; fluoride ions, when deposited and concentrated on the surface of austenitic stainless steel, can contribute to external stress ...
Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens
适用范围:<p>The procedures given are designed to remove corrosion products without significant removal of base metal. This allows an accurate determination of the mass loss of the metal or alloy that occurred d...
实施日期:2003-10-01
实施日期:1998-04-10
Standard Test Methods for Chemical Analysis of Thermal Insulation Materials for Leachable Chloride,Fluoride,Silicate,and Sodium Ions
适用范围:<p>Research has demonstrated that in addition to the halide ion chloride; fluoride ions, when deposited and concentrated on the surface of austenitic stainless steel, can contribute to external stress ...
实施日期:2011-05-15
实施日期:1998-04-10
Standard Practice for Determining the Susceptibility of Stainless Steels and Related Nickel-Chromium-Iron Alloys to Stress-Corrosion Cracking in Polythionic Acids
适用范围:<p>This environment provides a way of evaluating the resistance of stainless steels and related alloys to intergranular stress corrosion cracking. Failure is accelerated by the presence of increasing a...
实施日期:1998-04-10
Standard Practice for Making and Using U-Bend Stress-Corrosion Test Specimens
适用范围:<p>The U-bend specimen may be used for any metal alloy sufficiently ductile to be formed into the U-shape without mechanically cracking. The specimen is most easily made from strip or sheet but can be ...
实施日期:1997-04-10
请选择需要导出的字段:
请选择需要导出的字段:
知识产权声明 | 服务承诺 | 联系我们 | 客户服务 | 关于我们
网络出版服务许可证:(署)网出证(京)字第072号 互联网药品信息服务资格证书号:(京)-经营性-2016-0015 信息网络传播视听节目许可证 许可证号:0108284
万方数据标准管理系统V2.0 证书号:软著登字第11198474号
京ICP证:010071 京公网安备11010802020237号 京ICP备08100800号-1
客服电话:4000115888 客服邮箱:service@wanfangdata.com.cn 违法和不良信息举报电话:4000115888 举报邮箱:problem@wanfangdata.com.cn 举报专区:https://www.12377.cn
万方数据知识服务平台--国家科技支撑计划资助项目(编号:2006BAH03B01)©北京万方数据股份有限公司 万方数据电子出版社